Dettagli:
|
| Composizione materiale: | 80% Meta-Aramide + 20% Para-Aramide | Peso: | 70-90 GSM |
|---|---|---|---|
| Larghezza: | 150cm | Dopo il tempo di bagliore: | 0.8s |
| lunghezza danneggiata: | 4,5 CM | Processo: | tessuto non tessuto agugliato |
| Evidenziare: | 4.5 Cm Damaged Length Aramid Felt,0.8s After Glow Time Aramid Felt,70-90 gsm Meta Aramid Felt |
||
Aramid Needle Punched Felt Item: Aramid Felt Width: 150 cm Weight: 70–90 gsm Composition: 80% Meta Aramid + 20% Para Aramid Process: Needle punched nonwoven Description This aramid felt is manufactured by needle punching process, blended with 80% meta-aramid and 20% para-aramid staple fiber. Meta-aramid provides excellent inherent flame retardancy and thermal stability, while para-aramid brings outstanding tensile strength and tear resistance. The material will not melt or
Persona di contatto: Mr. Jack
Telefono: +86-18220501709
Fax: 86-512-52010711